Request a Quote
News

Moisture Sensitivity Levels: What Each Rating Means for Your Build

A moisture sensitivity level tells you how long a part can stay out of its dry bag before reflow. This guide explains each rating, the floor life behind it, and what to do when the clock runs out.

Home / News / Moisture Sensitivity Levels: What Each Rating Means for Your Build

November 2026

What Is a Moisture Sensitivity Level?

A moisture sensitivity level, or MSL, is a rating from 1 to 6 that tells you how long a plastic packaged surface mount part can sit in factory air after its dry bag is opened, before reflow soldering. The rating is assigned by the part maker under the classification standard published jointly by IPC and JEDEC. A higher number means a shorter safe time out of the bag, not a tougher part.

Plastic packages absorb moisture from the air, so a part that looks dry can hold enough water inside to cause damage when heated. The MSL tells the buyer and the line how much time they have.

The STM32F429ZIT6, a 144 pin LQFP microcontroller from STMicroelectronics, carries MSL 3, so it can stay out of its dry bag for 168 hours at or below 30°C and 60% relative humidity. For the buyer, the rating sets the build schedule: an MSL 5a reel must be finished within a day, while an MSL 3 reel gives the line a week.

How Long Can Each MSL Rating Stay Out of the Bag?

Floor life is the maximum time a part may stay out of its dry bag, counted from the moment the bag is opened until reflow, at or below 30°C and 60% relative humidity; MSL 1 uses 85%.

MSL ratingFloor lifeWhat it means in practice
MSL 1UnlimitedNo time limit, no dry pack needed
MSL 21 yearRecord the bag open date
MSL 2a4 weeksTrack cumulative open time
MSL 3168 hours, or 7 daysMost common rating
MSL 472 hours, or 3 daysPlan kitting and reflow inside 3 days
MSL 548 hours, or 2 daysKeep exposure records by lot or reel
MSL 5a24 hours, or 1 dayUse within one day
MSL 6Time printed on the labelBake before every use

Floor life is cumulative: every minute out of the bag counts. The clock pauses when parts return to dry storage below 5% relative humidity. The soak used to classify a part is its floor life plus a 24 hour allowance for the time the maker needs between baking and sealing the bag, which is why an MSL 3 part is soaked for 192 hours in classification but rated for 168 hours on the label.

Why Does Moisture Damage a Part in Reflow?

Moisture damage happens in the reflow oven. A plastic package left in humid air absorbs water into the mold compound around the die. During reflow the package heats quickly, the trapped water turns to steam, and the pressure has nowhere to go. The result is a crack in the package body or a separation between the die and the mold compound, a failure the industry calls popcorning.

The damage is not always visible. A cracked part can pass a visual check, solder onto the board, and fail weeks later in the field. The cost of ignoring floor life is rework, a stopped line, a missed ship date, and a field failure traced back to a reel that sat open too long.

What Is Inside a Dry Pack?

Parts rated MSL 2 to 6 ship in a dry pack: a sealed moisture barrier bag holding the parts, a desiccant pack, a humidity indicator card, and a caution label on the outside. MSL 1 parts do not need a dry pack.

The humidity indicator card is the quickest check in the system. Its spots change color from blue to pink when the humidity inside the bag passes set levels, at minimum 5%, 10%, and 60% relative humidity. Blue means the bag stayed dry. Pink means the parts need a bake.

The caution label carries the facts the line needs: the MSL rating, the peak body temperature, the floor life, the bake information, and the bag seal date. A sealed dry pack keeps a minimum shelf life of 12 months from the bag seal date below 40°C and 90% relative humidity.

What Should You Check When a Dry Pack Arrives?

Check the pack before it goes into stores. First, the bag should be sealed, with no puncture, tear, or open seam. Second, read the caution label and confirm the MSL, the floor life, and the bag seal date. Third, read the humidity indicator card while the parts are still in front of you. Fourth, confirm the date code and lot code on the parts match the label and the delivery documents, using the same checks in our guide to reading date codes and lot codes.

Record three facts: the bag seal date, the open date, and the indicator card reading. The open date starts the floor life clock. If any check fails, hold the parts and ask the supplier. A bag past its seal date is a question, not a rejection: if the card still reads dry, the parts can be used, and if the card reads wet, bake first.

What Happens When Floor Life Runs Out?

An expired floor life does not scrap the parts: bake them before reflow. Baking drives the absorbed moisture out of the package body, and a baked part starts with a fresh floor life clock. The bake time and temperature come from the bake table in the handling standard, and depend on package thickness, the MSL rating, and whether the parts stay in their carrier tape. As one example, a 1.0 mm thick MSL 3 part bakes for 8 hours at 125°C out of its tape, and 8 days at 40°C left in its tape. Keep total bake time above 90°C under 96 hours across the life of the part.

For a short overrun, drying can be enough. Parts rated MSL 2 to 4 that have been out for 12 hours or less can have the clock reset by drying in a dry cabinet for five times the exposure time. For MSL 5 to 5a, the limit is 8 hours out and ten times the exposure time in the cabinet. Longer than that, bake instead.

What Should You Ask Your Supplier About MSL?

Ask for the MSL before you place the order, not when the parts arrive. The rating decides the packaging you should expect, the floor life your line must plan around, and whether a bake needs to be booked. Ask for the bag seal date and the indicator card reading with the delivery, and a label photo on large orders.

Ask how the parts will ship. Original factory dry packs arrive sealed with desiccant and a card inside, and a repack for a smaller quantity should be a fresh dry pack with new desiccant and a new card, not a reel dropped into a plain bag. If the parts were baked before shipping, ask for the bake record: how long, at what temperature, and how much floor life is left. When you are ready to send the list, our BOM Kitting page takes the part numbers and quantities and returns a consolidated quotation for each line.

What Do Buyers Ask About Moisture Sensitivity Levels?

What does MSL 3 mean?

MSL 3 means the part can stay out of its dry bag for 168 hours, or 7 days, at or below 30°C and 60% relative humidity. It is the most common rating for packaged chips.

Does every part have an MSL rating?

No. The rating applies to moisture sensitive surface mount parts in plastic packages. Hermetic ceramic packages and most chip passives sit at MSL 1.

Can floor life be extended?

Yes. A dry cabinet below 5% relative humidity pauses the clock, and a bake resets it. For a short exposure, drying for five times the exposure time, or ten times for MSL 5 to 5a, can reset the clock without a bake.

What should I do if the humidity indicator card reads pink?

Bake the parts before reflow and do not rely on the original floor life. A pink spot means the humidity inside the bag passed the level marked on the card.

Written by Casey Xia

Casey Xia handles component sourcing enquiries at Potrgo, covering BOM quotation, shortage lines, and alternatives screening. These articles collect the checks and decisions behind that work. More about the author · Casey Xia on LinkedIn